Instable arc
The tungsten electrode gets oxidised and
tern at the end of welding.
The electrode melts
Default coming from the
tungsten electrode
Too important gas flow
rate
Welding zone
Default coming from
post-gas or the gas has
been stopped
prematurely.
Polarity error
Use a tungsten electrode with the
adequate size
Use a well prepared tungsten
electrode
Reduce gas flow rate
Protect welding zone against air
flows
Increase post-gas duration
Check
and
tighten
connections.
Wait
until
electrode
cools
down
stopping the gas.
Check that the earth clamp is really
connected to +
all
gas
the
before