ATTENTION
Leaking connection caused by faulty welding
▶ The pipe to be welded must be kept in a tension-free position
during the welding procedure and the cooling-down phase.
▶ Air draughts through the pipe interior must be avoided.
1
Connect the electrofusion tool to the mains voltage.
✓ <Mains connection> LED display
(see figure A,
2
Connect the connecting cable for electrofusion coupling to
the electrofusion coupling, electrofusion tape for anchor
point or electrofusion coupling with integrated thermal fuse.
✓ <Ready for welding> LED display
(see figure B,
3
Press the start button.
✓ <Welding procedure> LED display
the <Ready for welding> LED display
(see figure C,