No welding current.
The wire jams (after the rollers).
The welding bead is porous
The arc produces a lot of sparks
No gas flow at the end of the
torch.
28
NEOPULSE 270-T1 / 270-T2 / 300
Bad connection to the mains supply.
Bad earth connection.
Torch trigger inoperative.
Guide wire sheath crushed.
Wire jammed in the torch
No capillary tube.
Wire speed too fast
The gas flow rate is not sufficient.
Gas bottle empty.
Gas quality unsatisfactory.
Air flow or wind influence.
Gas nozzle dirty.
Poor quality wire.
Work-piece in bad condtion. (rust,
etc...)
No gas connected
Arc voltage too low or too high.
Bad earth connection.
Insufficient gas flow.
No gas connection
Bad gas connection.
Check the mains connection and ensure the
supply is 400 V (3PH).
Check the earth cable (connection and
clamp condition).
Check the torch trigger / replace torch
Check the sheath and torch body.
Clean or replace.
Check the presence of capillary tube.
Reduce the wire speed
Adjust flow range 15 to 20 L / min.
Clean the work-piece.
Replace
Replace
Prevent drafts, protect welding area.
Clean or replace the gas nozzle.
Use suitable WIRE for MIG-MAG welding.
Clean the metal before welding.
Check that the gas is connected to the
generator
See welding settings.
Check the earth cable (connection and
clamp condition)
Adjust the gas flow.
Check that the gas pipe is plugged to the
correct connector.
Check the gas connection at the welding
machine. Check the flowmeter and the
solenoid valves.
EN