Operating Instructions and Parts Manual
Troubleshooting Chart (Continued)
Symptom
Spray not uniform
(spitting)
Poor pattern
Overheating
Poor air flow
Spray tip clogs
Troubleshooting Chart - Finish Quality
Symptom
Orange Peel
(Rough rolling
appearance similar to
an actual orange
peeling)
Runs and sags
Pin-holing and solvent
pops
Fish eye
Blistering
Lumpy, coarse sur face
Mottled surface finish
• Weather conditions can cause unsatisfactory results when spraying some coatings.
• High humidity prolongs set, and cure times.
• High temperatures decrease set, and cure times.
• Cold temperatures extend set, and cure times.
• Variations in temperature, and humidity can cause variations in finish quality.
• Coating manufacturers can recommend additives to resolve some of these problems, and should be contacted for assistance
with particular problem resolutions.
Possible Cause(s)
1. Material too thick
2. Wrong nee dle / nozzle assembly
3. Cup seal leak ing
4. Loose pack ing
5. Material not properly mixed or
im prop er ly filtered
1. Material buildup on nozzle or air cap
2. Worn nee dle / nozzle
3. Clogged air cap
4. Material not properly mixed or
im prop er ly filtered
Clogged filter
1. Clogged filter
2. Air flow con trol improperly ad just ed
1. Im prop er ma te ri al flow adjustment
2. Cup seal leak ing
3. Wrong nee dle / nozzle
Possible Cause(s)
1. Material drying too fast
2. Gun too far from surface
3. Material too thick
1. Material too thin
2. Moving gun too slow
3. Ex ces sive material flow
4. Gun too close to surface
1. Trapped solvents
2. Pig ment settling
3. System contamination
Pos si ble silicone con tam i na tion
1. Mois ture in / on surface
2. In com pat i ble top coats or under-coats
Dirt on surface
1. Too much thinner
2. Poor spray technique
Corrective Action
1. Check ma te ri al viscosity (Thin per instructions)
2. Change to prop er nee dle / nozzle
3. Tighten cup, replace seal or check valve
4. Adjust or re place packing
5. Strain paint
1. Clean nozzle and air cap
2. Re place
3. Clean
4. Strain paint
Replace
1. Re place filter
2. Adjust air flow control
1. Adjust ma te ri al control
2. Replace cup seal
3. Change to prop er nee dle / nozzle
Corrective Action
1. Use a slower solvent or add a re tard ing agent
2. Move gun closer to surface
3. Thin material per thin ning in struc tions
1. Add ma te ri al to increase thickness
2. Move gun more quickly
3. Turn material control knob clock wise to reduce flow
4. Move gun further from surface
1. Apply material in lighter coats al low ing solvents time to
evaporate
2. Pos si ble bad material
3. Thor ough ly clean all parts
Use sol vent to clean all parts and work surfaces
1. Dry sur face
2. Make sure coatings are compatible
Thoroughly clean surface
1. Reduce thinner
2. Refer to "Operation" for spraying instructions
7