Problem
The welding pearl is
very narrow and bulky.
The welding pearl is
too wide.
The weld has low
penetration.
The weld has too
penetration.
If after all the recommended actions have been carried out the problems persist,
18
ENGLISH
Cause
• Welding current is too low.
• Welding speed is too fast.
• Welding current is too high.
• Welding speed is to slow.
• The arc is too long.
• Welding speed is too slow.
• The arc is too long.
• Welding current is too high.
• Welding speed is to slow.
• The arc is too long.
contact a
Troubleshooting
Solution
• Increase the speed and current to the micro wire.
• Move the torch slower and / or make circular
movements or zig zag movements with the nozzle.
• Diminish the micro wire current and speed .
• Move the torch faster and / or make less circular
movements or zig zag movements with the nozzle.
• Correct the distance between the nozzle and the
work piece (from 0.3" to 0.4").
• Increase the speed and current to the micro wire.
• Correct the distance between the nozzle and the
work piece (from 0.3" to 0.4").
• Decrease the speed and current to the micro wire.
• Move the torch faster and / or don't make circular
movements or zig zag movements with the nozzle.
• Correct the distance between the nozzle and the
work piece (from 0.3" to 0.4").