Final sintering

For the sintering, use only the Ceramill Argotherm high-tem-
perature furnace with protective gas connection (please also
refer to Ceramill Argotherm Operating Instructions).
NOTE:
▷ Pay attention that no pearls are jammed in the interdental spaces
or located in the crown cavities!
NOTE:
Faulty sintering results!
▷ To ensure proper sintering results, pay attention to the correct
arrangement of the sintering aids. Please also refer to the
Ceramill Argotherm Operating Instructions.
▷ Perform the final sintering of the frames in the Ceramill Argotherm.
▪ Program duration: approx. 5 hours
▷ Upon completion of the program, remove the sintering aids using
pliers.