MMA:
START-UP
A. Unpacking
Unpack all items from the package and ensure that all items, specified within the
scope of the delivery are present.
B. Work environment
It is necessary to ensure well ventilation within the working area. The device is cooled
by the fan which ensures cooling for all internal subassemblies of the device. (Tip! The
guards must be installed in such way that the vent holes could be located at the front
side of the device) In order to leave some space for cleaning and cooling, the device
should be located within the distance of at least 15 cm (from each side) from other
objects. If the device is not efficiently cooled, the make-time decreases.
C. Conduits connection
Each device is equipped with feeder cable which supplies it with electric voltage. If the
device is connected to the current source with the voltage exceeding supply rated
voltage or improper phase is connect, it may result in serious damage of the machine.
The device which has been damages in such course does not subject to repair under
the warranty terms.
D. WIG-WELDING
The handle has to be take by the hand. Unto the black closing cap. Next, it is necessa-
ry to insert wolframic electrode into the collet. Next put the housing onto the collet
and tighten the holder head (Nozzle).
34
EN
1 –MMA electrode holder
2 – workpiece
3 – mass clamp
Rev. 28.04.2022
INSTRUCTION OF OPERATION
TIG-welding
Clearing the station before welding.
The TIG-welding is very sensitive about the surface (which is to be welded) contami-
nation. For this reason, before welding you have to remove rests of paints and greases
as well as the oxidized layer from the surface which will be welded.
DC TIG-welding
Connect the gas hose to the gas to welder supply socket.
Connect the gas hose to the welding gun and to the argon supply (to the gun)
socket.
Connect weld piece to the mass clamp in welder, outlet (+).
Connect the welding handle plug to the arc and argon control rod.
Gas test: Check the connection of the electric supply and switch on the volta-
ge. Open the valve (regulator) of bottle with argon and switch on flow meter. Gun
switch-key has to be pressed and you have to select an appropriate gas flow. The
inflow switch-key has to be released and the gas inflow will be automatically stop-
ped after several seconds. In case of using the high frequency ignition, the wolframic
electrode has to be retracted 2-3 mm from the weld piece. Next, after switching on
the switch-key, the arc will be triggered. The switch off will result in the reduction of
electric current intensity and the arc will no longer be active. The blowing shaft can
not decay before the electric arc switch off. Gas must cool down the fusion weld as
it will not become oxidized. After finishing the welding process, you have to switch
off the argon supply button on the bottle and the welder supply. Pulling the electric
supply plug when the electric supply switch is on is prohibited.
Manual welding with the electrode
Connect the E-Hand conduit to the negative pole (-).
Set the current intensity regulator at the proper intensity (the impulse current
intensity regulator is in lower position). Select current in accordance with empiri-
cal formula: I=40d, where d is the electrode diameter.
Positive and negative connection during the welding process.
The welder has to be connected to the electric supply socket and turn main
switch on. The control lamp will light.
It is necessary to bring the attention to the relative intensity of welding current
and the relative welder's make-time.
The overloading may result in damages. You can avoid this.
After finishing the device operation, it is necessary to leave the device for cooling
and then – switch off the supply.
MAINTENANCE
The gun has to be checked for wear, cracks or bare conduits. All worn elements have
to be repaired or replaced before next operation of the device. Strongly worn gun
nozzle may result in the decrease of welding speed, voltage drop and uneven material
cutting line. The gun nozzle strongly worn symptom is the extended or too big hole.