MIG-MAG WELDING
• GMAW/MIG-MAG Manual
Settings
Designation
Wire speed
Voltage
Self
Pre-gas
Post gaz
• Standard MIG-MAG/GMAW (Dynamic STD)
The Standard mode allows high quality welding on most ferrous materials such as steel, stainless steel, but also copper and its alloys, titanium... The
many possibilities of current and gas management allow you to perfectly control your welding operation, from the priming to the final cooling of your
weld bead.
Settings
Designation
Thickness
Speed
Current
Arc length
Welding positioning
Self
Pre-gas
Approach speed
Hot Start
Cold current/Back-
ground current
Pulse frequency
Duty cycle ratio
Crater Filler
Post gaz
PULSFEED 4W
Adjustable
settings
1 - 22 m/min
Quantity of filler metal deposited and indirectly the welding intensity.
10 - Umax
Sets the welding power.
Smoothes more or less the welding current. To be adjusted according to the welding
-4 > +4
position.
0 - 25 secs.
Torch purge time and to protect the area with gas before ignition
Duration for which gas is released after the arc has stopped. It protects the weld pool
0 - 25 secs.
and the electrode against oxidisation when the metal is cooling down.
Adjustable
settings
The synergy allows for fully automatic settings. Adjusting the thickness
0.1 - 5.5 mm
automatically sets the right voltage and wire speed.
1 - 22 m/min
Quantity of filler metal deposited and indirectly the welding intensity.
The welding current is adjusted according to the type of wire used and the material to
15 - Imax
be welded.
Used to adjust the distance between the end of the wire and the weld (voltage adjust-
-6 > +6
ment).
-
-
Smoothes more or less the welding current. To be adjusted according to the welding
-4 > +4
position.
0 - 25 secs.
Torch purge time and to protect the area with gas before ignition
Progressive wire speed. Before the arcing, the wire arrives slowly to create the first
50 - 200 %
contact without causing a jolt.
The Hot Start is an overcurrent during generated during the arcing phase to prevent
50 - 200 %
the wire from sticking. It is adjustable in intensity (% of welding current) and time
0 - 5 secs.
(seconds).
50 - 100 %
Second welding current known as «cold» welding current
0.1 - 2 Hz
Pulse frequency
20 - 80 %
In pulsed mode, sets the hot current time in relation to the cold current time.
This current treshold when stopped is a phase after the current downslope.
50 - 100 %
It is adjustable in intensity (% of welding current) and time (seconds).
Duration for which gas is released after the arc has stopped. It protects the weld pool
0 - 25 secs.
and the electrode against oxidisation when the metal is cooling down.